Open the CIPO recordAbstract From the Canadian patent
The catalyst comprises a mixture of hydrocracked residual asphaltene and metal-doped coke. The catalyst is produced by mixing an oil-soluble metal compound catalyst precursor (e.g. Mo or Ni soap) with heavy oil containing asphaltene and hydrocracking the mixture, producing solid coke as a byproduct. The residual asphaltene fraction in the hydrocracked oil is then precipitated for example with, n-pentane. The mixture of solid coke and precipitated asphaltene is separated and used as the catalyst for hydrocracking a new batch of non-hydrocracked oil. The coke and asphaltene mixture provides as effective a catalyst as the original metal soap catalyst precursor. The coke and asphaltene mixture …
Read the whole patent
Listed from its CIPO record in Patent Yard's archive of Canadian patents past their term. Its claims, description and drawings are in the CIPO record and on Google Patents, and the Claude kit works from them.
Why it's free to use
- Filed June 12, 1997 and granted June 5, 2001. A Canadian patent filed from October 1, 1989 lasts 20 years from filing, so its term ended June 12, 2017.
- A certificate of supplementary protection adds at most two years for a drug, so even that would have ended by June 12, 2019.
- We check Canadian rights only. A patent in its family in another country could still be in force: check its family on Google Patents.
Timeline
Timeline From CIPO dates
Sources & verification
Official CIPO records
Everything on this page comes from the CIPO record linked above. Contains information licensed under the Open Government Licence – Canada.