Method of repairing damages in superalloys
CA 1324242 C · Owner: Miller, Jule A. · Inventors: Lee, Jack W.; Iovene, Michael A.; Miller, Jule A.
Overview
Its claims, description and drawings are in the Canadian Patents Database.
Open the CIPO recordAbstract From the Canadian patent
A method of repairing damages in a superalloy component is disclosed wherein existing brazed joints and protective coatings are not harmed. The method entails the use of a silicon-free metal mixture comprising (i) a low melting alloy having a liquidus below the temperature to be used to deposit the metal mixture (ii) an alloy melting above about 2100°F and (iii), optionally nickel. The resultant repair has a solidus temperature of at least 1950°F, preferably at least 2000°.
Read the whole patent
Listed from its CIPO record in Patent Yard's archive of Canadian patents past their term. Its claims, description and drawings are in the CIPO record and on Google Patents, and the Claude kit works from them.
Why it's free to use
- Granted November 16, 1993. A Canadian patent filed before October 1, 1989 lasted 17 years from grant, so its term ended November 16, 2010.
- We check Canadian rights only. A patent in its family in another country could still be in force: check its family on Google Patents.
Timeline
Timeline From CIPO dates
Sources & verification
Official CIPO records
Everything on this page comes from the CIPO record linked above. Contains information licensed under the Open Government Licence – Canada.